红柱石砖 |
项 目\指 标 |
SHZ-135 |
SHZ-140 |
SHZ-145 |
SHZ-150 |
Al2O3,% |
≥65 |
≥65 |
≥65 |
≥75 |
Fe2O3,% |
≤1.5 |
≤1.5 |
≤1.5 |
≤1.0 |
显气孔率, % |
≤20(22) |
≤20(22) |
≤20(22) |
≤19(20) |
体积密度, g/cm3 |
≥2.55 |
≥2.55 |
≥2.60 |
≥2.65 |
常温耐压强度, MPa |
≥60(50) |
≥60(50) |
≥70(60) |
≥80(60) |
0.2MPa荷重软化开始温 度,℃ |
≥1600 |
≥1600 |
≥1600 |
≥1650 |
耐火度,℃ |
≥1790 |
≥1790 |
≥1790 |
≥1790 |
蠕变率 (0.2MPa,20-50h),% |
1350℃ ≤0.2 |
1400℃ ≤0.2 |
1450℃ ≤0.2 |
1500℃ ≤0.2 |
|
| 注:括号内数据为单重大于12.5kg 的砖。 |
|