项目 | 刚玉-莫来石砖 | 莫来石-刚玉砖 | 再烧电熔莫来石砖 | 莫来石砖 | 莫来石砖 |
RTSA-CM-90 | RTSA-CM-80 | RTSA-CM-75 | RTSA-CM-70 | RTSA-CM-62 | |
Al2O3 % ≥ | 90 | 80 | 75 | 70 | 62 |
SiO2 % ≥ | 8 | 18 | 23 | 25 | 36 |
Fe2O3 % ≤ | 0.3 | 0.5 | 0.5 | 0.5 | 0.8 |
体积密度g/m3 ≥ | 2.90 | 2.70 | 2.65 | 2.55 | 2.48 |
显气孔率 % ≤ | 18 | 19 | 14 | 16 | 17 |
常温耐压强度 Mpa ≥ | 100 | 80 | 100 | 90 | 80 |
荷重软化温度(0.2Mpa,0.6%),℃ ≥ | 1700 | 1650 | 1700 | 1630 | 1450 |
重烧线变化(1600℃×3h), % | ±0.3 | ±0.3 | ±0.2 | ±0.2 | ±0.2 |