| 项目 | 铬刚玉砖 | ||||
| RTSA-CrC-5 | RTSA-CrC-12 | RTSA-CrC-20 | RTSA-CrC-30A | RTSA-CrC-30B | |
| Cr2O3 % ≥ | 5 | 12 | 20 | 30 | 30 |
| Al2O3+Cr2O3 % ≥ | 93 | 93 | 93 | 93 | / |
| Cr2O3+Al2O3+ZrO2 % ≥ | / | / | / | / | 93 |
| Fe2O3 % ≤ | 0.3 | 0.3 | 0.3 | 0.3 | 0.3 |
| 体积密度g/m3 ≥ | 3.10 | 3.20 | 3.40 | 3.40 | 3.45 |
| 显气孔率 % ≤ | 18 | 18 | 18 | 18 | 18 |
| 常温耐压强度 Mpa ≥ | 100 | 100 | 100 | 100 | 100 |
| 荷重软化温度 (0.2Mpa,0.6%),℃ ≥ | 1700 | 1700 | 1700 | 1700 | 1700 |
| 重烧线变化(1600℃×3h), % | ±0.3 | ±0.3 | ±0.3 | ±0.3 | ±0.3 |